Properties
Thermocollant winged ride in cotton, slightly scraped - average thickness.
Application
Areas of application
Small parts, such as passes and blouse cuffs and shirts. Average to thick fabrics.
Treatment
1. The woven spinning, like all Vlieseline entrances, is always cut in the longitudinal direction, following the direction of the wire
2. Place the overlapping, on the coated side on the back of the outer fabric, cover it with a damp canvas and iron in jolts for about 12 seconds. Do not drag the iron.
3. After fixing, let the parts cool for about 30 minutes flat to allow membership to stabilize.
Benefits
• cannot deform